Loading...
Menu
Trending Products
Vibrating Gold Sluice
Vibrating Gold Sluice
SF type flotation machine
SF type flotation machine
BF type flotation machine
BF type flotation machine
JJF type flotation machine
JJF type flotation machine
BS-K type flotation machine
BS-K type flotation machine

Hydraulic Radial Jig

Hydraulic Radial Jig has many advantages compared with ordinary jigger: large jigging area, strong processing capacity; because the jigging tank body is fan-shaped, it is conducive to the recovery of fine-grade materials; compact structure, centralized feeding, separation of minerals occupies a small space, and it is suitable for use on mining ships; because of the use of hydraulic transmission, the transmission mechanism is simplified and saves power.

 

Need a plan quote or proposal? Available for free 24/7!

Contact: +8619914754015 (WeChat/WhatsApp)

Submit your inquiry for a tailored solution.

 

Model: {{ product.model }}
weight: {{ product.weight }} Kilogram

{{ variable.name }} : {{ variable.values[selectedVariantsIndex[variable_index]].name }}

{{ value.name }}
Product Inquiry
Hydraulic Jig | Gravity Separation Equipment for Alluvial Gold Roughing and Early Recovery of Coarse Native Gold

The DYTA-7750 hydraulic jig is a high-efficiency gravity concentrator fully optimized and upgraded from traditional equipment. It employs an innovative hydraulic-mechanical drive system: a cam pushes the main hydraulic cylinder, converting electrical energy into mechanical and hydraulic energy to generate powerful vertical pulsations in the jig cone. Fitted with an electromagnetic speed-regulating asynchronous motor, it allows stepless adjustment from 0 to 90 strokes per minute, perfectly suiting the separation of alluvial gold, alluvial tin, diamonds, tungsten, manganese and hematite. With its large jigging area, excellent throughput, outstanding energy and water savings and compact structure, it has become the preferred choice for roughing on gold dredges and land mines. In gold ore processing it handles the most valuable and yet most economical stage of the flowsheet: directly recovering already liberated coarse native gold (density 15.6–19.3) before the ore enters the grinding circuit and before alluvial gold becomes locked in slime. If that gold follows the ore into the ball mill, it is merely ground repeatedly in vain, flattened into flakes and clayified fines, and finally lost with cyclone overflow and tailings. The hydraulic jig concentrates these particles in the 0.5–25 mm range in a single pass by means of an asymmetrical sawtooth-wave pulsating flow, making it the part of overall gold recovery with the best return on investment. GoldProcessingPlant specializes in gold mining and processing equipment and processes, and offers selection of all 10 models DYTA7750-3 to DYTA7750-12, matching of area and chamber count, sector launder, screen and bed configuration, skid mounting and dredge-deck adaptation, plus complete-line quotations for "washing——screening——jig roughing——centrifugal concentration——table cleaning——flotation scavenging——thickening and water recirculation".

DYTA-7750 hydraulic jig——gravity separation equipment for alluvial gold roughing and coarse native gold recoveryGoldProcessingPlant DYTA-7750 hydraulic jig (hydraulic-mechanical drive system · multi-chamber jig cones · sector launder · stepless regulation by electromagnetic speed-regulating asynchronous motor)

Product Overview

The DYTA-7750 hydraulic jig is a high-efficiency gravity concentrator fully optimized and upgraded from traditional equipment. It employs an innovative hydraulic-mechanical drive system: a cam pushes the main hydraulic cylinder, converting electrical energy into mechanical and hydraulic energy to generate powerful vertical pulsations in the jig cone. Fitted with an electromagnetic speed-regulating asynchronous motor, it allows stepless adjustment from 0 to 90 strokes per minute, perfectly suiting the separation of alluvial gold, alluvial tin, diamonds, tungsten, manganese and hematite.

With its large jigging area, excellent throughput, outstanding energy and water savings and compact structure, it has become the preferred choice for roughing on gold dredges and land mines, with outstanding application results.

The difficulty of gravity gold recovery can be summed up in three words: large, fine and variable. First, throughput is enormous: alluvial, residual-colluvial and oxidized alteration-zone wash ores usually contain pebbles, slime and water measured in tens to hundreds of millimetres, and need a roughing machine that can "swallow and run", not a small refined cleaning unit; roughing on a dredge deck also requires one machine to handle the whole feed with a limited allowance of fresh water and power. Second, gold particle size spans a huge range: the same alluvial gold pile contains millimetre-scale flaky gold and coarse native gold, but also sub-0.074 mm ultrafine gold and encapsulated gold; the former fears being carried away by the rising current and the latter being lost with slime, and a symmetrical sinusoidal pulsation can hardly serve both ends. Third, ore and feed rate fluctuate violently: the grade and slime content of alluvial gold change rapidly along the ore body, and dredges see almost constant flow and density variation as excavation advances, water level and screen condition change; the machine must be able to adjust stroke and frequency online and steplessly rather than stopping to change cams or pulleys. And gold is more sensitive than other minerals to "early recovery": native gold has high density (15.6–19.3) and good ductility; once in the grinding circuit and subjected to repeated grinding, it is flattened into flakes and hard-to-settle fines that neither jigs nor tables can retain, forming the hardest part of total gold loss to recover.

The value of the DYTA-7750 lies precisely here: it replaces traditional mechanical transmission with a hydraulic drive that delivers large energy steadily and controllably to the jig cone, generating a fast-rise, slow-fall asymmetrical sawtooth-wave pulsating flow: the rising phase rapidly lifts and loosens the bed, while the falling phase prolongs stratification and produces gentle suction, so dense gold particles pass first through the bed interstices and settle at the bottom while gangue is carried away by the flow, markedly improving fine heavy-mineral recovery. Strokes of 20, 25 and 30 mm and stepless 0–90 strokes/min frequency allow the setpoint to be changed when the ore, size distribution or density changes. The large-scale design with a sector launder and 3–12 chambers in series brings the jigging area of a single machine to 9.9–39.6 m² and capacity to 50–300 t/h. The nine-chamber model has a total power of only 11.6 kW, and under-screen makeup water is just 1/4 of a traditional jig, saving up to 55% of electricity and 60%–70% of water; for water- and power-scarce mountain and plateau alluvial gold mines and dredges with limited fresh-water allowance, these are the economic indicators that decide project viability.

In a gold processing plant, the hydraulic jig typically appears in six positions: (1) roughing of alluvial gold and dredges: washed and screened material is jigged directly to obtain gold rough concentrate in one pass, the most characteristic duty of the series; (2) early recovery of coarse native gold in hard-rock gold plants: installed in classification ahead of the ball mill or as a grinding-circuit bypass to extract already liberated coarse gold and avoid idle grinding and clayification; (3) main recovery of the gravity section: forming a ternary system of "jig roughing——centrifugal scavenging——table cleaning" with the automatic centrifugal concentrator and 6-S shaking table; (4) cleaning of jig rough concentrate: rough concentrate goes to the 6-S table for high-grade gold, reducing the load of later cyanidation and flotation; (5) reuse of old tailings dumps and slags: recovering residual gold from historical tailings; (6) comprehensive recovery of associated heavy minerals: concentration of heavy minerals from tin-gold, tungsten-gold, manganese-gold and hematite-gold ores. A permanent magnetic separator is recommended at the inlet to remove drill bits, rods and liner fragments, together with an electromagnetic vibrating feeder or reciprocating feeder for uniform feeding so that a too-thick or too-thin bed does not disrupt stratification. For hard-rock gold it integrates into the gravity separation circuit for hard-rock gold ore, while alluvial gold follows the alluvial gold processing flowsheet.

Working Principle

The DYTA-7750 hydraulic jig consists mainly of an electromagnetic speed-regulating asynchronous motor, cam mechanism, main hydraulic cylinder and hydraulic system, jig cone (diaphragm), sector launder, screen plate and heavy-mineral bed, under-screen water system, and feeding and discharge devices. In operation, the motor rotates the cam, which pushes the main hydraulic cylinder in reciprocating motion, transforming electrical energy into mechanical and hydraulic energy; the cylinder then drives the jig cone to produce powerful, controllable vertical pulsations. The up-and-down movement of the cone creates rising and falling currents together with a particle bed in the chamber, and the material completes the sequence of loosening——stratification——separation according to density difference: denser native gold and heavy minerals pass through the bed into the underflow (heavy product), while light gangue (quartz, feldspar, density about 2.65) leaves with the rising current and overflow, achieving concentration.

The key to efficiency lies in the shape of the pulsation curve. Traditional jigs are directly driven by an eccentric cam and produce an almost sinusoidal flow with symmetrical rise and fall and high acceleration peaks: the bed is "violently lifted and struck"; although coarse heavy minerals can settle, fine and flaky gold is lifted by the strong rising current and escapes with tailings before passing through the bed. Through hydraulic damping and cam-profile design, the DYTA-7750 emits a sawtooth pulsation curve: fast rise lifts the whole bed in a very short time and loosens it completely, eliminating agglomeration and segregation dead zones; slow fall keeps the bed loose longer during settling, offering gold particles sufficient "separation channels", while gentle suction in the falling phase "draws" fine heavy minerals from above down to the bed bottom. This rise-fall asymmetry is the physical reason for the notable improvement in fine heavy-mineral recovery and why it outperforms traditional models on "fine, flaky and light" heavy minerals such as alluvial gold and cassiterite.

Hydraulic-mechanical drive system and sawtooth-wave pulsation chamber structure of the hydraulic jigHydraulic-mechanical drive and jigging chamber of the hydraulic jig: the cam pushes the main cylinder, the cone pulsates up and down, and the screen with its bed forms the asymmetrical sawtooth flow; stroke 20/25/30 mm and frequency 0–90 strokes/min are adjusted online by feed size and density

There are three adjustment dimensions at the core of field operation: (1) stroke (20, 25, 30 mm) determines the degree of bed loosening and "throw height"; use a large stroke for coarse, pebbly material and a small one for fine, slimy material; (2) frequency (0–90 strokes/min, nominal working range 50–85) determines the number of stratifications per unit time; finer classes prefer higher frequency, coarser ones lower; (3) under-screen makeup water (1–3 m³/t of ore, pressure ≥0.10 MPa) determines bed suspension height and rising-current intensity, and is the most direct lever for controlling gold loss in tailings. The combination of the three covers a wide range of conditions from coarse alluvial gold to fine auriferous sands, and the electromagnetic speed-regulating motor allows stepless online adjustment without stopping to change parts when the ore changes.

Sector launder and chambers in series are another structural feature determining capacity: the launder widens progressively from inlet to outlet, with low inlet velocity favouring settling of coarse heavy particles and gradually adjusted velocity and bed state at the outlet, forming a natural gradient of "roughing——scavenging"; connecting 3–12 chambers in series, each with its own cone and bed, allows separate adjustment and observation: coarse gold concentrates in the first chambers while fine gold continues separating in the latter ones, guaranteeing large capacity while optimizing fine recovery. It should be stated honestly that jigging is a method that operates by density and is very effective for already liberated coarse and medium native gold, but cannot handle gold encapsulated in quartz or fully oxidized gold in ultrafine dispersed form: that portion must be recovered by flotation with BF/JJF/XCF-KYF cells or by cyanidation after grinding; therefore the jig's role in the plant is "early recovery and roughing", not the sole method for the whole flowsheet.

Advantages and Features

  • Extreme energy savings and leading cost
    • Up to 55% electricity saving: the nine-chamber model has a total power of only 11.6 kW, greatly reducing operating cost. Benefit for gold: the largest power consumption in a plant is crushing and grinding; every kW saved in the gravity section is pure profit. For remote alluvial gold points and dredges relying on diesel generators, 55% saving rewrites cost per tonne and fuel consumption, restoring economic viability to low-grade alluvial deposits.
    • 60%–70% water saving: under-screen makeup water is only 1/4 of a traditional jig, easing supply pressure, especially in arid areas. Benefit for gold: alluvial gold washing is the plant's "big water drinker"; cutting makeup water by 60%–70% means smaller intake works, pump power and tailings-pond volume. In arid mountains, plateaus and ecologically sensitive zones, an inclined-plate thickener and settling pond enable a closed wash-water circuit with over 85% recirculation and less gold-slime loss in discharge.
  • Advanced drive and efficient separation
    • Hydraulic drive system: stable operation, robust power, simplified structure and far higher reliability than mechanical transmission. Benefit for gold: hydraulic transmission replaces multi-stage gears and eccentric shafts; oil absorbs impact loads and greatly extends bearing and transmission life. On dredges and mountain plants, where "maintenance is inconvenient and every stop loses ore", availability equals production; stable pulsation keeps bed thickness constant and prevents instantaneous flow peaks from washing away coarse and flaky gold.
    • Sawtooth pulsation curve: generates an asymmetrical fast-rise, slow-fall flow that optimizes bed loosening and stratification and notably improves fine heavy-mineral recovery. Benefit for gold: flaky and fine gold are the main loss source of traditional sinusoidal jigs; the slow-fall phase and gentle suction extend the settling window for gold, retaining in the rough concentrate that gold which was "visible but unrecoverable", directly lifting overall recovery and feed grade.
  • Large capacity and wide adaptability
    • Large-scale design: big jigging area with sector launder guarantees high capacity while optimizing fine recovery. Benefit for gold: with 9.9–39.6 m² chamber area and 50–300 t/h, one machine can swallow the whole feed of a medium alluvial plant or a dredge, reducing machine count, feeding points and conveyor belts, and thus fine-gold loss and dust at every transfer.
    • Stepless regulation: frequency is freely adjustable between 0 and 90 strokes/min for different ores and size compositions. Benefit for gold: alluvial gold grade, slime and flow fluctuate constantly; when the mining face or season changes (frozen ground or flood season), the operator adjusts frequency and stroke online to stabilize the bed without stopping to change cams. Together with an electromagnetic vibrating feeder this forms a three-parameter closed loop of "flow——frequency——makeup water", stabilizing the amount of coarse gold recovered before grinding.
  • Rugged, compact, stable and reliable
    • Compact structure: small footprint, especially suited to mobile platforms with limited space such as gold dredges. Benefit for gold: on a dredge, deck area and load are hard constraints; at equal capacity a smaller footprint allows more jigging area and more complete roughing. Mountain plants and retrofits also benefit: small foundation, little civil work, direct installation under existing washing and screening structures, shorter construction and lower investment.
    • Easy maintenance: humanized design, low failure rate, simple installation, operation and daily maintenance, adapted to harsh conditions. Benefit for gold: wear parts concentrate in the screen, rubber liner and bed, whose replacement does not require lifting the whole machine; good hydraulic sealing and low dust-protection demand suit the wet, abrasive, low winter-temperature conditions of alluvial gold, ensuring continuous dredge and plant production.

How to Choose Between the Hydraulic Jig, Traditional Jig, Centrifugal Concentrator and 6-S Shaking Table

Four machines are often confused in the gravity section of gold: the DYTA-7750 hydraulic jig generates sawtooth pulsations with a hydraulically driven cone, operates by density difference, and specializes in large-capacity roughing and early recovery of 0.5–25 mm coarse fractions; the traditional jig (mechanical cam/diaphragm) also operates by density but with symmetrical sinusoidal pulsation, higher power and water use and limited fine recovery; the automatic centrifugal concentrator enhances fine heavy-mineral concentration through strong centrifugal force (tens of times gravity) at high rotation speed, specializing in sub-0.074 mm ultrafine gold and clayified gold; the 6-S shaking table uses asymmetrical reciprocating bed motion plus differential cross-flow transport, specializing in narrow-size feed and directly delivering high-grade gold. The four form a series relationship of "jig roughing first, centrifugal back-up scavenging, table cleaning last", not a choice among four alternatives.

Item Hydraulic jig DYTA-7750 Traditional jig (cam/diaphragm) Automatic centrifugal concentrator 6-S shaking table
Concentration principle Hydraulically driven cone, asymmetrical sawtooth flow (fast rise, slow fall) + gentle suction Eccentric cam or mechanical diaphragm, symmetrical sinusoidal flow High-speed rotating drum generating strong centrifugal force to enhance settling of fine heavies Asymmetrical bed reciprocation + differential cross-flow, two-dimensional stratification by size and density
Advantageous size Mainly 0.5–25 mm coarse and medium particles, with fine and flaky gold clearly superior to sinusoidal models 2–25 mm coarse particles, limited recovery of fines and flaky gold Fines below 0.074 mm, clayified gold and gravity-tailings scavenging 0.074–2 mm narrow size range; coarse sand/fine sand/slime need different beds
Capacity per unit 50–300 t/h, 10 models and 3–12 chambers Lower; equal output needs more units and larger area Low; units added in number and bed needs periodic washing Low; requires strictly classified feed and several parallel units
Energy and water use 55% power saving (nine chambers, 11.6 kW) and 60%–70% water saving, makeup 1–3 m³/t Higher consumption; makeup water about 4 times this machine Needs higher feed pressure and wash water; medium power use High water use per tonne; needs circulation pumps
Regulation Stroke 20/25/30 mm + stepless 0–90 strokes/min, online adjustment and repeatability Limited range and complex operation; changing condition requires stop and mechanical change High automation, but batch concentration and discharge Need to change bed and adjust slope and water by size; many parameters
Product and enrichment ratio Continuous discharge of rough concentrate (heavy product), medium ratio, large-scale recovery Continuous concentrate discharge, normal ratio, large fine loss Very high enrichment ratio, direct high-grade gold and rich middlings Direct high-grade gold, well-defined middling and tailing bands
Wear and maintenance Screen, rubber liner, bed and hydraulic seals; simple structure and easy maintenance Cam, diaphragm, bearings and transmission with heavy wear and much maintenance Drum, wear parts and distributor; needs periodic bed washing Bed, connecting rod and springs; many wear parts but low unit cost
Most suitable gold scenario Alluvial gold and dredge roughing, large land-based alluvial plants, early coarse-gold recovery in hard-rock plants, old tailings reprocessing Existing old plants, simple treatment of rich coarse ore Scavenging of gravity and jig tailings, ultrafine and clayified gold recovery Cleaning of jig/centrifugal rough concentrate, final grade upgrading, fine narrow-size separation

Practical criterion: for large capacity, 0.5–25 mm size and continuous roughing with early recovery of coarse native gold, choose the DYTA-7750 hydraulic jig; an already built old plant treating only rich coarse ore with no retrofit budget may stay with a traditional jig, but once power and water costs are counted the payback for replacing it with a hydraulic jig is usually short (foundation and piping can be reused); for ultrafine gold, clayified gold and gravity-tailings scavenging, choose the automatic centrifugal concentrator; for obtaining high-grade gold, the 6-S shaking table. The normal GoldProcessingPlant configuration is "run-of-mine ore → screw washer washing and desliming → trommel or vibrating screen screening and pebble removal → vibrating or reciprocating feeder for uniform feeding → permanent magnetic separator → DYTA-7750 jig roughing → rough concentrate to 6-S table for high-grade gold → jig tailings to centrifugal concentrator for ultrafine gold scavenging → tailings to BF/JJF/XCF-KYF cells for residual gold scavenging → inclined-plate thickener for thickening and water recirculation". In hard-rock plants a jigging bypass is added on the classified product of the ball mill → hydrocyclone/spiral classifier to extract liberated coarse gold early. The hydraulic jig fulfils the "early coarse-gold recovery gate", clearly separated from the centrifugal concentrator's "fine back-up gate", the table's "grade-upgrading gate" and flotation's "residual sulphide-gold gate", and is integrated into the combined gold ore processing flowsheet.

Technical Parameter Table

The DYTA-7750 series comprises 10 models, DYTA7750-3, -4, -5, -6, -7, -8, -9, -10, -11 and -12 (3 to 12 chambers), with jigging area of 9.9–39.6 m², capacity of 50–300 t/h and main motor power of 5.5–15 kW, covering test lines and small alluvial points through medium alluvial and hard-rock gold plants, dredges and thousand-tonne-scale large plants.

Model and parameter DYTA7750-3 DYTA7750-4 DYTA7750-5 DYTA7750-6 DYTA7750-7 DYTA7750-8 DYTA7750-9 DYTA7750-10 DYTA7750-11 DYTA7750-12
Jigging area (m²) 9.9 13.2 16.5 19.8 23.1 26.4 29.7 3.3 36.3 39.6
Capacity (t/h) 50-75 66-100 78-125 100-150 116-175 132-197 150-200 166-245 182-270 200-300
Main motor power (kW) 5.5 7.5 7.5 7.5 11 11 11 15 15 15
Weight (kg) 6000 8000 10000 12500 14200 15800 17500 18000 19200 21000

Common parameters for the whole series:

Item Parameter Gold note
Stroke (mm) 20, 25, 30 Coarse and pebbly alluvial gold: 30 mm; fine with much slime: 20 mm; stroke determines bed loosening
Frequency (strokes/min) 50-85 (range 0–90) Fines: higher frequency; coarse: lower; stepless online regulation by electromagnetic motor
Feed size (mm) <25 Oversize pebbles must be removed by heavy trommel or vibrating screen or they damage bed and screen
Under-screen makeup water (m³/t) 1-3 Main lever of bed suspension height; only 1/4 of a traditional jig
Under-screen water pressure (MPa) ≥0.10 Needs clean-water pump and stabilized piping; recommend combining with inclined-plate thickener recirculation
Hydraulic station motor power (kW) 0.55 Same across the series; together with the main motor forms total installed power

Parameter notes: (1) capacity and area are reference values calculated for <25 mm feed, reasonable stroke and frequency and a proper bed configuration; actual output varies with bulk density (normally 2.6–3.0 t/m³ for gold ore, with more slime and water in alluvial gold), size composition, feed density and target enrichment ratio, so selection should be calculated from real conditions with a 15%–20% margin; (2) the unit of jigging area in the original header was m³; as a physical "area" it should be m², which is how it is shown on this page; (3) the jigging area of DYTA7750-10 is shown as 3.3 in the original data, inconsistent with the arithmetic progression of 3.3 m² per chamber across the series (9.9/13.2/16.5/19.8/23.1/26.4/29.7/…/36.3/39.6); it is suspected to be a typographical error for 33.0, but this page reproduces the original figure without alteration; verify the nameplate with the engineer before signing; (4) regarding frequency, 0–90 strokes/min in the description is the regulation range of the electromagnetic speed-regulating motor, while 50-85 in the table is the nominal working interval; actual adjustment is stepless within the range according to size and bed state; (5) the "11.6 kW total power of the nine-chamber model" in the advantages is an operating reference for a specific configuration, whereas main motor power (11 kW for DYTA7750-9) and hydraulic motor (0.55 kW) in the table are installed powers——different concepts; electrical distribution and costing are based on the confirmed configuration; (6) overall dimensions and foundation load are not in the source material (the nine-chamber model already weighs 17500 kg); for dredge decks and skid mounting, provide load capacity and installation limits and the engineer will issue a foundation drawing and counterweight calculation; we do not invent parameters.

Model Recommendations for Gold Plants

Plant scale and condition Suggested model Configuration points
Test line, small alluvial points and skid units (50–75 t/h) DYTA7750-3 9.9 m², main motor 5.5 kW, weight 6000 kg; compact and easy to transport on a skid; small stroke (20 mm) and high-precision feeding recommended; on shutdown route remaining bed material to the settling pond
Early recovery of coarse native gold in small and medium alluvial and hard-rock plants (66–125 t/h) DYTA7750-4/-5 13.2/16.5 m², 7.5 kW; 25 mm stroke suits both coarse and fine; upstream trommel for pebbles and magnetic separator are mandatory to protect screen and bed
Roughing on dredges and large land-based alluvial plants (100–200 t/h) DYTA7750-6/-7/-8/-9 19.8–29.7 m², 7.5–11 kW; chambers in series form a roughing——scavenging gradient; size by deck load and fresh-water allowance, with under-screen water closed circuit and thickener recirculation
Thousand-tonne alluvial plants, old tailings reprocessing and large dredges (166–300 t/h) DYTA7750-10/-11/-12 36.3–39.6 m², 15 kW; one unit absorbs the whole feed, reducing transfers and fine-gold loss; a complete gravity room with centrifugal concentrator and 6-S table is recommended
Water- and power-scarce mountain and plateau zones, diesel-generation points Any model + recirculation system Here the 55% power saving and 60%–70% water saving are amplified; configure pond/inclined-plate thickener for closed wash-water circuit and calculate pump head and winter frost protection
Detail of the multi-chamber sector launder and jig cone of the hydraulic jigDetail of the DYTA-7750 multi-chamber sector launder and jig cone: each chamber has its own cone and bed with separately adjustable stroke and frequency, forming a natural roughing-to-scavenging gradient from inlet to outlet and combining high capacity with fine recovery

Applicable Minerals and Use Scenarios

Range of applicable minerals:

  • Precious metals: alluvial gold (and coarse native gold recovered early in the grinding circuit of hard-rock plants)
  • Non-ferrous metals: alluvial tin, tungsten ore
  • Ferrous metals: manganese ore, hematite
  • Non-metallic minerals: diamonds, barite

Typical gold scenarios:

  • Roughing on dredges (gold, tin, etc.): compact structure, small footprint and low power and water consumption; the preferred option where deck space and fresh-water allowance are doubly restrictive, with continuous discharge of gold rough concentrate.
  • Large land-based alluvial plants: 50–300 t/h per unit; with sector launder and series chambers it directly absorbs the whole feed after washing and screening, reducing machine count and transfer losses.
  • Recovery of fine and ultrafine heavy minerals (alluvial gold, cassiterite): asymmetrical sawtooth pulsation extends the stratification window and retains in the heavy product the fine and flaky gold that sinusoidal models cannot recover.
  • Reuse of old tailings dumps and slags: historical auriferous tailings and slags are rewashed, screened and jigged to recover residual gold with little investment and quick results, while eliminating the environmental risk of the dump. See gold recovery from tailings and precious metals flowsheet.
  • Early recovery of coarse native gold in hard-rock plants: a jig is installed in classification ahead of the ball mill or as a circuit bypass, extracting liberated coarse gold before it enters the mill and avoiding idle grinding, flaking and fine loss in overflow.
  • Preconcentration of heavy minerals in auriferous polymetallic ore: associated tin-gold, tungsten-gold, manganese-gold and hematite-gold minerals are first concentrated by gravity and then routed to flotation or cyanidation according to their nature, reducing reagent and equipment load downstream.
Hydraulic jig installed in an alluvial gold roughing and dredging operationHydraulic jig installed in an alluvial gold roughing and dredging operation: qualified material (<25 mm) is uniformly fed, rough concentrate goes to the 6-S table for cleaning and tailings to the centrifugal concentrator for ultrafine gold recovery

Customization Services

  • Custom chamber count and jigging area: 3 to 12 chamber models selected by capacity, size and target recovery; area and launder width can be customized with regard to dredge deck dimensions and plant civil limits.
  • Stroke, frequency and electrical configuration: standard electromagnetic speed-regulating asynchronous motor (0–90 strokes/min), with optional variable-frequency control and centralized control cabinet, interlocked with feeder and pump for a three-parameter closed loop of flow——frequency——makeup water.
  • Sector launder and screens: aperture, open area and launder expansion angle selected by size to optimize bed stability and fine recovery; reinforced coarse screen offered for highly abrasive auriferous quartz sand.
  • Bed and rubber liner: bed density and size selected by separation density difference (iron-borate or barite beds commonly used), with wear-resistant rubber inner lining balancing precision and service life.
  • Feeding, discharge and launders: uniform distribution box, overflow weir and discharge launders for heavy product (concentrate) and tailings; heavy product connects directly to the 6-S table and tailings to the centrifugal concentrator, avoiding transfer losses.
  • Skid and dredge adaptation: integral skid unit, damping and tie-down structure, deck load and counterweight calculation, and anti-overturning layout drawing, adapted to dredge and mobile-unit vibration and changing conditions.
  • Water system and recirculation: clean-water pumps, stabilized piping and valves sized for 1–3 m³/t of ore and pressure ≥0.10 MPa, with an inclined-plate thickener and settling pond for closed wash-water circuit and gold-slime recovery.
  • Full-process service: selection calculation, civil and foundation drawings, installation guidance, commissioning and operator training, with complete supply of screw washer, heavy trommel, vibrating screen, electromagnetic vibrating feeder, reciprocating feeder, permanent magnetic separator, jaw crusher, spring cone crusher, impact crusher, ball mill, hydrocyclone, spiral classifier, automatic centrifugal concentrator, 6-S shaking table, BF/JJF/XCF-KYF flotation cells and inclined-plate thickener for the whole line, all integrated into the gold processing equipment supply.
General layout of the gravity concentration workshop and auxiliary piping of the hydraulic jigGeneral layout of a GoldProcessingPlant gravity concentration workshop: the hydraulic jig is arranged together with feeding, iron removal, table cleaning, centrifugal scavenging and thickening with water recirculation, with unified interfaces avoiding mismatches between suppliers

Why Choose Our DYTA-7750 Hydraulic Jig

  • Hydraulic sawtooth drive for higher fine-gold recovery: asymmetrical fast-rise, slow-fall pulsation optimizes bed loosening and stratification, retaining fine and flaky alluvial gold in the rough concentrate and directly raising overall gold recovery——a core advantage hard for traditional sinusoidal jigs to match.
  • 55% less electricity, 60%–70% less water, leading cost per tonne: the nine-chamber model has only 11.6 kW and makeup water of 1/4 of traditional models; for dredges and alluvial points with diesel power and limited fresh water, the cost advantage directly decides the project's profitability threshold.
  • Large sector launder + 3–12 chambers in series, one machine replacing several: 9.9–39.6 m² and 50–300 t/h; one unit performs the roughing-to-scavenging gradient, reducing feeding points, belts and fine-gold loss, with a compact structure and small footprint for dredges and mountain plants.
  • Complete-line supply and process calculation: GoldProcessingPlant does not merely sell machines: it runs gravity tests on ore samples, calculates bed, stroke and frequency, and delivers the material balance and equipment selection for the whole "washing——screening——jigging——centrifugation——tabling——flotation——thickening and recirculation" flowsheet, avoiding disparate interfaces and badly coupled flows between suppliers.

Frequently Asked Questions

What is a hydraulic jig and what role does it play in gold processing?

A hydraulic jig is a gravity concentrator that generates pulsation through a hydraulic-mechanical drive system: a motor rotates a cam that pushes the main hydraulic cylinder, converting electrical energy into mechanical and hydraulic energy to move the jig cone powerfully up and down; particles complete the loosening——stratification——separation cycle in rising and falling vertical currents according to their density difference: dense native gold settles at the bottom as heavy product while gangue leaves with the overflow. In gold processing it performs five functions: (1) alluvial gold and dredge roughing, delivering rough concentrate in one pass, the most characteristic duty of the series; (2) early recovery of coarse native gold, extracting already liberated gold (density 15.6–19.3) before the mill to avoid flaking by idle grinding and fine loss; (3) main gravity recovery, forming a roughing——scavenging——cleaning ternary system with the centrifugal concentrator and 6-S table; (4) reprocessing of old tailings and slags to recover residual gold; (5) preconcentration of associated heavy minerals in tin-gold, tungsten-gold and manganese-gold ores, reducing later flotation and cyanidation load.

What is a sawtooth pulsation curve and how does it differ from a traditional sinusoidal one?

The curve describes the velocity-time shape of the vertical flow (or screen) movement in the chamber. A traditional jig is directly driven by an eccentric cam or diaphragm and produces an almost sinusoidal motion with symmetrical rise and fall and high acceleration peaks: the bed is "violently lifted and struck", with nearly equal loosening and stratification times; coarse heavies can settle, but fine and flaky gold is lifted by the strong rising current and escapes with tailings before passing through the bed. The DYTA-7750 hydraulic jig hydraulically damps and profiles the cam to emit a sawtooth wave: fast rise lifts the whole bed and loosens it completely, eliminating agglomeration and dead zones; slow fall keeps the bed loose longer during settling, offering gold sufficient separation channels, while gentle suction "draws" fine heavies to the bottom. In practical terms: notable improvement in fine heavy-mineral recovery, more stable concentrate grade and, with gentler flow peaks, the bed is not "punctured" and coarse gold is not carried away. That is the physical reason for its superiority on "fine, flaky and light" heavy minerals such as alluvial gold and cassiterite.

Why does the hydraulic jig save 55% electricity and 60%–70% water?

Electricity saving comes from simplification of the transmission chain and effective use of energy: the hydraulic-mechanical drive replaces multi-stage gears, eccentric shafts and high-inertia parts with a cam and main cylinder; there are fewer links and mechanical losses, and the hydraulic system adapts output to bed resistance. The nine-chamber model consumes only 11.6 kW, 55% less than traditional models. Water saving comes from the change in pulsation shape and feeding mode: the fast-rise, slow-fall sawtooth wave loosens the bed sufficiently with a smaller rising current, without large flows needed to lift it by force; hence under-screen makeup water is only 1/4 of a traditional jig (1–3 m³/t, pressure ≥0.10 MPa), giving 60%–70% total water saving. For the plant this means: (1) smaller intake works, pumping power and cable sections, so water and power quotas cease to be a bottleneck; (2) less discharge and tailings volume, lowering environmental cost; (3) with an inclined-plate thickener and settling pond, wash-water recirculation exceeds 85%, reducing gold-slime loss in discharge.

How to choose between DYTA7750-3 and -12? Which model suits 100 or 200 t/h?

Three factors correspond: target capacity + feed size + space and load conditions. The whole series covers 9.9–39.6 m² and 50–300 t/h. DYTA7750-3 (9.9 m², 50-75 t/h, 5.5 kW, 6000 kg) suits test lines and small alluvial points. DYTA7750-4 (13.2 m², 66-100 t/h, 7.5 kW, 8000 kg) and -5 (16.5 m², 78-125 t/h, 7.5 kW, 10000 kg) suit small and medium plants; for 100 t/h choose -4 or -5 (choose -5 if an upper-limit margin of 15%–20% is wanted). DYTA7750-6 to -9 (19.8–29.7 m², 100-200 t/h, 7.5–11 kW, 12500–17500 kg) are the main range for dredges and medium alluvial plants. For 200 t/h, DYTA7750-9 (150-200 t/h) or -10 (166-245 t/h) is recommended, the latter more comfortable with high slime, moisture and variable feed. DYTA7750-11/-12 (36.3/39.6 m², 182-270/200-300 t/h, 15 kW) serve thousand-tonne plants, tailings reprocessing and large dredges. Two warnings: (1) table capacity assumes <25 mm and reasonable stroke and frequency; with high slime, moisture and variable bulk density calculate from real conditions; (2) on a dredge deck verify weight (-9 already 17500 kg, -12 21000 kg) and dynamic load, with load and counterweight calculation by the engineer.

How are the 20/25/30 mm stroke and 0–90 strokes/min frequency adjusted? What effect do they have on recovery?

Stroke determines bed loosening and throw height; frequency determines the number of stratifications per unit time; both must match feed size and density. For coarse and pebbly alluvial gold (10–25 mm) use a large stroke (30 mm) and lower frequency so the bed loosens wholly without compacting; for fine, slimy material (0.5–3 mm) use a small stroke (20 mm) and higher frequency, with gentle high-frequency pulsation and suction so fine gold passes through the bed; for medium size, 25 mm. Under-screen water (1–3 m³/t) is the third lever: too little compacts the bed and fine gold cannot descend; too much lifts gold into tailings, the most common cause of "gold loss" in alluvial plants. Tuning criterion: first fix stroke by size, then adjust frequency and water with tailings and concentrate grade as feedback until you find the combination of "loose bed, visible gold grains in concentrate and no visible native gold in tailings", and mark the position; restore from the marks when the mining face or season changes (freezing or flood). Since the electromagnetic speed-regulating motor adjusts speed steplessly and online, all this is done without stopping or changing mechanical parts, key to adapting to violent changes in gold ore.

Why must feed size be below 25 mm? What happens with oversize and high slime?

Jigging relies on a stable, uniform bed, and <25 mm is the condition to maintain its structure. With oversize: large pebbles and blocks entering the chamber first strike and break the screen, compact the bed and block apertures, causing uneven under-screen water distribution and local "fountains" that carry gold directly to tailings; second, they jam between cone and launder and damage the cone and hydraulic system; third, they reduce effective settling area, lowering both capacity and recovery. Therefore install a heavy trommel or vibrating screen upstream to remove oversize and use a vibrating/reciprocating feeder for uniform feeding (fluctuating flow thins and thickens the bed and disorders stratification). With high slime: clay and fines wrap gold, increase pulp viscosity and form a "slime blanket" on the bed that hinders separation, while much fine slime leaves with overflow carrying fine gold. The solution is a double-screw washer to scrub and deslime before jigging and an inclined-plate thickener to treat overflow and recover fine gold; in reprocessing slime-rich auriferous tailings also control feed density to avoid "slime-wrapped gold". A permanent magnetic separator at the inlet is also recommended to remove drill bits, rods and liner fragments before they damage screen and bed.

Can it recover fine and flaky gold? Will gold be washed away?

That is precisely the strength of the series, but its limits should be understood. It can recover: already liberated native gold or coarse crystals, with density 15.6–19.3 against quartz (~2.65) and feldspar, which under fast-rise, slow-fall sawtooth pulsation passes through the bed first and settles; flaky gold, with its large specific area, was easily lifted and was the main loss of sinusoidal jigs, but the slow-fall phase and gentle suction greatly improve its settling window and, with a smaller stroke and less under-screen water, it is effectively recovered. It cannot recover: encapsulated gold in quartz and fully oxidized gold in ultrafine dispersion, which offer no density difference and require grinding followed by flotation with BF/JJF/XCF-KYF cells or cyanidation. Will gold be washed away? Under normal conditions no: native gold settles quickly and mostly enters the underflow (heavy product); only two risks exist: (1) too much makeup water lifting fines and flakes into overflow, so strictly keep 1–3 m³/t and watch tailings grade; (2) direct discharge of overflow and wash water losing gold slime——route it to a settling pond or inclined-plate thickener and never directly to tailings. GoldProcessingPlant can provide a gold-loss diagnostic table and recirculation plan at the selection stage.

Is the hydraulic jig suitable for dredges and mobile units? Is installation and maintenance complicated? What are the wear parts?

Very suitable. Dredge roughing is the native scenario of the series: compact structure and small footprint ideal for space-limited mobile platforms; moreover 55% less electricity and 60%–70% less water answer exactly the double constraint of onboard power and fresh water; hydraulic transmission runs smoothly and oil absorbs impact loads, adapting to hull vibration and feed fluctuation. On land, skid units, mountain plants and retrofits also benefit: small foundation, little civil work and direct installation under washing and screening structures. Installation: the machine is of integral type and requires foundation and damping (nine chambers 17500 kg, twelve chambers 21000 kg, with load calculation), plus connection of the feed launder, under-screen water piping (≥0.10 MPa) and concentrate and tailings discharge launders. Easy maintenance is a design objective: low failure rate and humanized layout; daily points concentrate on screen, rubber liner, bed and hydraulic-system seals, oil level and quality; changing screen and liner does not require lifting the whole machine. Check bed state and water pressure each shift, hydraulic oil and fasteners weekly, and screen wear and open area quarterly. In cold mountain and plateau winters, protect the hydraulic system against freezing and drain water on shutdown to avoid ice blockage and oil emulsification.

How are the hydraulic jig, centrifugal concentrator, 6-S table and flotation combined? Where are they installed in the flowsheet?

The four divide work by size and operating target and are used in series, not as substitutes. The DYTA-7750 hydraulic jig handles roughing and early recovery of 0.5–25 mm coarse fractions, with large capacity and continuous concentrate discharge; the automatic centrifugal concentrator handles sub-0.074 mm ultrafine gold and clayified gold, with a very high enrichment ratio, and scavenges jig tailings for fine gold the jig did not retain; the 6-S shaking table handles cleaning, upgrading jig rough concentrate and centrifugal concentrate to high-grade gold (different beds for coarse sand/fine sand/slime and strictly classified feed); BF/JJF/XCF-KYF flotation cells handle sulphide-encapsulated gold and residual gold: gold in pyrite and arsenopyrite must be concentrated by flotation before roasting or cyanidation. The GoldProcessingPlant standard configuration is: run-of-mine ore → double-screw washer for desliming → heavy trommel/vibrating screen for classification and pebble removal → vibrating or reciprocating feeder for uniform feeding → permanent magnetic separator → DYTA-7750 hydraulic jig for roughing → rough concentrate to 6-S table for high-grade gold → jig tailings to centrifugal concentrator for scavenging → tailings to BF/JJF/XCF-KYF cells for residual gold scavenging → inclined-plate thickener for thickening and water recirculation. In hard-rock plants a jigging bypass is added on the classified product of the ball mill → cyclone/spiral classifier to recover coarse gold early; grinding fineness is set by the cyclone or classifier and the jig receives only qualified sizes, so they do not interfere. When residual gold goes to flotation, the whole sequence is integrated into the gold flotation flowsheet.

How much does a hydraulic jig cost? What information is needed for a quotation?

The DYTA-7750 price depends on model and chamber count (3–12), jigging area, screen and bed configuration, level of electrical and frequency control, skid or dredge mounting, and whether it is supplied as a set with other equipment. From the operating-cost side, the nine-chamber model has only 11.6 kW and under-screen water of 1/4 of traditional models, saving 55% electricity and 60%–70% water, so electricity and water savings usually repay the price difference quickly. When requesting a quotation from GoldProcessingPlant, provide: (1) ore type (alluvial gold/residual-colluvial and oxidized zone/crushed hard-rock product/tailings reprocessing/gold associated with tin, tungsten, manganese and hematite); (2) size composition and maximum feed size (whether <25 mm, pebble and slime content); (3) target capacity (t/h) and daily operating hours; (4) bulk density, feed density and moisture; (5) current flowsheet and auxiliaries (whether washer, trommel, feeder, magnetic separator, table, centrifugal concentrator, flotation and thickener already exist); (6) installation conditions (ground foundation, mountain gradient, dredge deck dimensions and load, skid mounting); (7) available water and power (flow and head, voltage and whether diesel generation); (8) whether centralized frequency control, water closed circuit and complete-line design are required. GoldProcessingPlant engineers will then issue model selection, area and bed configuration, material balance and a complete-line quotation.


With its hydraulic sawtooth drive, large sector launder of 3 to 12 chambers and outstanding energy and water savings, the DYTA-7750 hydraulic jig offers a high-performance solution for alluvial gold roughing and early recovery of coarse native gold. GoldProcessingPlant can supply, according to your capacity, feed size, bulk density and slime and water content, selection of models DYTA7750-3 to -12, chamber, screen and bed configuration, and a complete line of washing——screening——jigging——centrifugation——cleaning——flotation——thickening and recirculation, integrated into the combined gold ore processing flowsheet.

Tell Us Your Capacity and Feed Size

GoldProcessingPlant engineers select models DYTA7750-3 to DYTA7750-12, area and chamber count, stroke and frequency, screen and bed configuration, and skid and dredge-deck adaptation

Free selection report for alluvial gold roughing and early coarse-gold recovery, capacity calculation by bulk density and slime and water content, sawtooth pulsation parameter tuning, gold-loss diagnosis, closed wash-water circuit and a complete-line quotation

Get Hydraulic Jig Selection and a Quotation

CONTACT US

To find out more about our products and solutions, please fill out the form below and one of our experts will get back to you shortly.

Nginx server needs to configure pseudo-static rules, click View configuration method