ball mill

GoldProcessingPlant provides professional solutions of ball mill in gold ore grinding. The equipment realizes the fine grinding of ore through the impact of steel balls to achieve the optimal particle size for mineral dissociation, which is especially suitable for the crushing and grinding operation of gold ore, and can significantly improve the grinding efficiency and the recovery rate of mineral processing.

 

Need a plan quote or proposal? Available for free 24/7!

Contact: +8619914754015 (WeChat/WhatsApp)

Submit your inquiry for a tailored solution.

 

Model: {{ product.model }}
weight: {{ product.weight }} Kilogram

{{ variable.name }} : {{ variable.values[selectedVariantsIndex[variable_index]].name }}

{{ value.name }}
Product Inquiry
Ball Mill | Core Grinding and Gold-Mineral Liberation Equipment for Gold Processing

The ball mill is the core grinding machine in a gold processing plant, reducing auriferous quartz veins, altered rock and silicified fracture-zone ores until gold minerals are liberated from the gangue. The rotating cylinder lifts steel balls that impact and grind the ore; the reduction ratio exceeds 300 and continuous dry or wet operation is supported, providing the grinding fineness required for flotation, gravity separation (centrifugal concentrator, jig, shaking table) and cyanide leaching. Two types are offered: grate type (forced discharge, large capacity) and overflow type (finer product, ideal for regrinding). GoldProcessingPlant advises on mill selection and circuit layout according to ore nature and tonnage, and the mills can be integrated into the combined gold ore processing flowsheet.

Grate-type and overflow-type ball mills in a gold processing plantGoldProcessingPlant ball mills installed at a gold operation (grate type / overflow type)

Product Overview

The ball mill is the key fine-grinding machine after initial fragmentation. Its rotating cylinder carries the grinding media (steel balls) that impact and grind material into very fine powder. In a gold plant, ore passes through a jaw crusher (coarse crushing) and a spring cone crusher (medium and fine crushing) before entering the mill: grinding fineness directly determines the degree of gold mineral liberation. Auriferous quartz veins and altered rocks are usually strongly silicified and very hard; under-grinding leaves gold locked in the gangue and unrecoverable, while over-grinding generates slime, raises tailings losses and increases energy consumption. The ball mill is also essential in mining, building materials, chemicals, power and metallurgy, grinding gold ore, cement clinker, silicates and refractories. It works in dry or wet grinding, with wet grinding predominant in gold plants.

Qualified pulp then passes to separation stages. GoldProcessingPlant can connect this machine to the gravity separation circuit for hard-rock gold ore, gold flotation process, CIP process, CIL process and gold recovery from tailings and precious metals flowsheet, as well as gold processing equipment list for a complete line, flexibly arranged according to their position in the flowsheet.

Working Principle

The work of a ball mill is divided into four stages: feeding, impact and grinding, staged fine grinding and discharge. The rotating cylinder carries steel balls that impact and grind the ore, progressively liberating gold minerals along the interface with silicified gangue.

  1. Feeding: the ball mill is a horizontal rotating cylindrical device. Crushed auriferous ore is fed uniformly into the first chamber through the hollow trunnion; in wet grinding, process water is added simultaneously to form pulp.
  2. Impact and grinding: the cylinder contains steel balls of various sizes as grinding media. Driven by the transmission, centrifugal force lifts the balls to a certain height, from which they fall in cascade by gravity. The falling balls produce strong impact and abrasive grinding on the auriferous ore, gradually liberating gold along the interface with silicified gangue.
  3. Staged fine grinding: after coarse grinding in the first chamber, material passes through a single partition wall into the second chamber, which normally carries smaller balls for finer grinding and control of feed size and gold liberation.
  4. Product discharge: pulp reaching the required fineness exits through the discharge grate (grate type, forced discharge) or overflows at the outlet end (overflow type, natural overflow), and is sent to the classifier, hydrocyclone, centrifugal concentrator and flotation cell to recover gold and reduce fine loss to tailings.
Cylinder, wear-resistant liner and grinding media of a ball millBall mill cylinder and wear-resistant liner——directly determining the grinding efficiency of auriferous ore

Main Structure and Characteristics

A ball mill consists of four parts: feeding, discharge, rotating body and transmission.

  • Feeding part: introduces auriferous ore uniformly and ensures stable feed to the grinding circuit.
  • Discharge part: includes the grate (grate type) or hollow trunnion (overflow type) to discharge ground pulp.
  • Rotating body: the core, formed by the cylinder, hollow trunnions and liners. Wear-resistant liners (stepped, wave or flat) inside protect the cylinder and improve ore grinding efficiency.
  • Transmission part: motor, reducer, pinion and girth gear, driving cylinder rotation through peripheral gear transmission.

Main characteristics:

  • Strong adaptability: dry or wet production, continuous operation and large capacity, suiting gold plants of different sizes.
  • High reduction ratio: above 300, with fineness easily adjusted to control the liberation size of gold.
  • Robust structure and reliable operation: cast-steel hollow trunnions, cast girth gear with machined teeth, key wear-resistant components and stable running.
  • Good sealing: supports negative-pressure operation, preventing dust escape and improving the plant working environment.
  • Multiple variants: by discharge system, the grate mill (forced discharge, larger capacity) and the overflow mill (natural overflow, finer product).

Choosing Between Grate and Overflow Types

Type Discharge system Product characteristics Typical gold processing application
Grate ball mill (MQG) Forced discharge through discharge grate Large capacity, high efficiency, little over-grinding Primary and secondary coarse and fine grinding in gold plants; main high-tonnage crushing and grinding line
Overflow ball mill (MQY) Natural overflow at the outlet end Finer particle size, more complete grinding Gold regrinding and fine grinding before flotation / cyanide leaching where high fineness is required (e.g. high -200 mesh percentage)

In a gold flowsheet, crushing normally uses a jaw mill plus spring cone crusher for coarse, medium and fine crushing; the grate mill handles main grinding and the overflow mill handles fine grinding and regrinding. Both form closed circuits with a classifier or hydrocyclone and supply qualified pulp to centrifugal concentrators, jigs and flotation cells.

Cylinder appearance of a grate ball mill in a gold plantGrate ball mill cylinder——peripheral gear transmission and cast-steel hollow trunnion

Technical Parameter Table

The table below lists main parameters of commonly used grate-type (MQG) ball mills. The plant can pre-select a model by tonnage and fineness, and GoldProcessingPlant engineers will refine the configuration according to auriferous ore properties, feed size and product fineness:

Model Cylinder speed (r/min) Ball load (t) Feed size (mm) Discharge size (mm) Capacity (t/h) Motor power (kW) Weight (t)
MQG900×900 38 1.5 ≤20 0.075-0.89 0.65-1.8 7.5 2.9
MQG1200×1200 32 3.8 ≤25 0.075-0.6 1.6-4.8 18.5 8.6
MQG1500×1500 27 8 ≤25 0.074-0.4 4-12 55 16.5
MQG1830×3000 21 27 ≤25 0.074-0.4 10-45 180 38
MQG2100×3000 19 38 ≤25 0.074-0.4 20-60 210 55
MQG2200×4500 18 60 ≤25 0.074-0.4 35-90 380 85
MQG2400×4500 17 75 ≤25 0.074-0.4 50-120 475 110
MQG2700×3600 16 85 ≤25 0.074-0.4 60-140 550 135

Gold selection recommendation: small hard-rock gold test lines can choose MQG900 to MQG1200; secondary grinding in medium auriferous quartz-vein plants commonly uses MQG1500 to MQG1830; for main grinding of large-scale altered-rock plants, grate mills MQG2200 or above are recommended, with MQY overflow mills for regrinding and fine grinding.

Reducer and large and small gears of a ball mill transmissionMill transmission: motor, reducer and peripheral girth gear drive the cylinder to rotate
Hollow trunnion and inlet and outlet ends of a grate ball millInlet and outlet ends and hollow trunnion: ensuring uniform feed and discharge of auriferous pulp

Why Choose Our Ball Mill

Five reasons, in summary:

  1. Adapted to gold liberation
  2. Wear resistance and lower consumption
  3. Robust and reliable structure
  4. Fineness easily adjusted
  5. Complete-line supply

Faced with the high silicified hardness of auriferous quartz veins and altered rock, we optimize the liner curve and ball gradation for complete liberation of gold minerals with less over-grinding. High-chromium alloy or rubber liners and optimized ball grading reduce steel and energy consumption per tonne; grinding cost is one of the main items in a plant budget, so saving consumption means increasing profit.

Cast-steel hollow trunnions, machined girth gear teeth and peripheral gear transmission ensure stable long-term continuous operation. With a reduction ratio above 300 and flexible discharge combined with classification, fineness can be placed in the optimum window for gold flotation and cyanide leaching.

Integrated supply with jaw crusher, spring cone crusher, centrifugal concentrator, jig and flotation machine, arranged together according to the combined gold ore processing flowsheet. GoldProcessingPlant provides complete crushing – grinding – separation solutions.

Installation and operation of ball mills in a gold processing plantInstallation and closed-circuit operation of GoldProcessingPlant ball mills in a gold plant

Frequently Asked Questions

What is a ball mill and what role does it play in gold processing?

It is the key fine-grinding machine after initial crushing: the rotating cylinder carries steel balls that impact and grind the ore. In a gold plant it grinds ore to liberate gold minerals from gangue and creates recovery conditions for flotation, gravity separation and cyanide leaching. Grinding fineness directly affects overall gold recovery.

What is the difference between grate and overflow ball mills, and how to choose?

The grate mill (MQG) discharges forcibly through a grate: large capacity and little over-grinding, suited to the main grinding line of primary and secondary coarse and fine grinding. The overflow mill (MQY) overflows naturally at the outlet: finer product, suited to regrinding and fine grinding before flotation / cyanidation. Choose by tonnage and the fineness required by the process.

What is the working principle of a ball mill?

Auriferous ore enters the first chamber uniformly through the hollow trunnion; the cylinder rotates and centrifugal force lifts the balls, which fall in cascade and generate impact and grinding on the ore. Material then passes the partition into the second chamber with smaller balls for finer grinding; qualified pulp exits through the grate (grate type) or the outlet end (overflow type).

What fineness is normally required for gold grinding and how is it controlled?

Flotation and cyanide leaching usually require 60%–90% passing 200 mesh (depending on the ore); finely disseminated gold needs higher fineness. Control is achieved by choosing grate or overflow type, adjusting ball gradation and cylinder speed, and operating in closed circuit with a classifier or hydrocyclone. GoldProcessingPlant determines target fineness through beneficiation tests.

Can it grind dry and wet? Which is used for gold?

Both are possible. Dry grinding is used mainly in cement and refractories; wet grinding predominates in gold processing, adding water to form pulp that facilitates subsequent classification, gravity separation and flotation while controlling fineness and reducing dust.

What are the wear parts of a gold ball mill and how long does the liner last?

The main wear parts are the cylinder liner, end-cover liner, hollow trunnion / feeder, pinion and girth gear, and balls. Liner life depends on ore silicified hardness and tonnage; high-chromium alloy or rubber liners significantly extend life and reduce steel consumption per tonne.

What faults are common and how are they handled?

The most common are excessive main-bearing temperature (check lubrication and cooling), abnormal cylinder vibration (check liner bolts and ball load), pulp leakage at the trunnion (check seals and liner wear) and abnormal gear noise (check meshing and lubrication). Regular lubrication and bolt-tightening inspections greatly reduce fault downtime.

What lubricant does a gold ball mill use and how is it maintained?

Main bearings and trunnions usually use a lubrication station with fluid oil or grease; pinion and girth gear are treated with gear oil. Maintenance consists of periodic oil replenishment and change, monitoring bearing temperature, tightening liner bolts and controlling ball consumption for timely replenishment, keeping the grinding circuit stable.

What size mill suits a 50 or 100 tonne-per-hour plant?

Tonnage and fineness together determine the model. As a reference, plants of several tens of tonnes per hour commonly use grate mills MQG1830×3000 to MQG2200×4500; at larger scale choose MQG2400 or above, or several units in parallel. Provide tonnage, feed size and target fineness and GoldProcessingPlant performs selection free of charge.

How much does a ball mill cost and what data are needed for a quotation?

Price depends on the model (grate or overflow, cylinder diameter and length), motor power and configuration. Provide plant tonnage, feed size, product fineness, ore nature (quartz vein, altered rock, etc.) and whether a classifier is required; GoldProcessingPlant engineers select the model and issue a quotation without cost.

As the core machine that achieves liberation of gold minerals, the ball mill stands out for mature technology, wide applicability and stable operation. The grate type prioritizes large capacity and efficiency in coarse and fine grinding; the overflow type suits regrinding with finer particle size. GoldProcessingPlant selects the optimal model and offers complete crushing – grinding – separation solutions according to your auriferous ore properties, tonnage and target fineness, along with the gold processing equipment list for complete-line supply.

Tell Us Your Gold Tonnage and Grinding Fineness

GoldProcessingPlant engineers select the grate / overflow ball mill model and arrange the grinding circuit

Free selection proposal and quotation, with complete-line supply of jaw crushers, spring cone crushers and centrifugal concentrators

Get Ball Mill Selection and a Quotation

CONTACT US

To find out more about our products and solutions, please fill out the form below and one of our experts will get back to you shortly.

Nginx server needs to configure pseudo-static rules, click View configuration method