6-S Shaking Table

Provide professional application solution of 6-S Shaking Table in gold ore gravity separation. This equipment realizes the precise separation of gold particles through the asymmetric reciprocating motion of the bed, which is especially suitable for the recovery of fine-grained gold ores, and can effectively improve the concentrate grade and recovery rate.

 

Need a plan quote or proposal? Available for free 24/7!

Contact: +8619914754015 (WeChat/WhatsApp)

Submit your inquiry for a tailored solution.

 

Model: {{ product.model }}
weight: {{ product.weight }} Kilogram

{{ variable.name }} : {{ variable.values[selectedVariantsIndex[variable_index]].name }}

{{ value.name }}
Product Inquiry
6-S Shaking Table | High-Precision Separator for Free Gold and Gravity Concentrate Cleaning in Gold Beneficiation

The 6-S shaking table is one of the core machines of gravity concentration, renowned for its extremely high separation precision and enrichment ratio, and is also the customary separator in gold plants for recovering free gold, native gold and fine gold particles. Through the combined action of gravity, water drag, deck friction and inertia, auriferous particles stratify and form radial bands by density and size, producing a high-grade gold concentrate and discardable tailings in a single pass. In gold beneficiation, the 6-S table is widely used for roughing, cleaning and scavenging of auriferous quartz veins, altered-rock deposits and placer gold; within the combined gold ore processing flowsheet it is often installed after the jig and centrifugal concentrator for final cleaning, forming coarse, medium and fine free-gold bands in one pass, reducing tailings losses and improving overall gold recovery. It offers three decks—coarse sand, fine sand and slime, and two configurations—left-hand and right-hand, making it an indispensable precision separator in concentrators. GoldProcessingPlant specializes in gold extraction equipment and processes, and can advise on table selection and gravity circuit layout according to your ore nature and capacity.

Actual photograph of a 6-S shaking table in a gold plant and the banding distribution on its deckGoldProcessingPlant: actual view of a 6-S shaking table in a gold plant (deck riffles·stroke adjustment mechanism·concentrate-band side)

Product Overview

The 6-S shaking table is one of the core machines of gravity concentration and stands out for its extremely high separation precision and enrichment ratio (concentrate grade / feed grade). Through the combined action of gravity, water drag, deck friction and inertial force, it stratifies particles and arranges them in bands by density and size, generating a high-grade concentrate and discardable tailings in a single pass. The machine has a very wide field of application: it suits tungsten, tin, tantalum, niobium, gold, silver, iron, manganese, chromium, titanium, coal and other metallic and non-metallic minerals, and can be used in roughing, cleaning and scavenging, making it an indispensable precision separator in the plant.

In gold beneficiation, the value of the 6-S table is especially notable: auriferous quartz veins, altered-rock deposits and silicified fracture zones, after primary jaw crusher crushing, secondary and fine spring cone crusher crushing and liberation grinding in a ball mill, present the gold as free gold or concatenated particles in the pulp with pronounced density differences—ideal feed for table gravity concentration. The table efficiently concentrates liberated coarse and medium native gold at the concentrate end while banding gangue and auriferous slime, preventing loss of gold minerals before flotation or cyanidation. For placer gold and old tailings reprocessing, the table is usually the last line of scavenging and cleaning, recovering once more the ultrafine gold that escaped sluices, gold carpets and jigs, directly affecting overall gold recovery and plant profitability.

Working Principle

Auriferous pulp is fed through the inclined feed trough of the deck and simultaneously subjected to cross wash water. Under the combined effect of gravity, cross-flow water drag, inertia and friction generated by the asymmetric reciprocating motion of the deck, particles stratify by density and size.

  • Heavy mineral particles (native gold, heavy sand minerals) settle in the lower layer, where deck friction acts more strongly and they travel a longer longitudinal path, being pushed toward the concentrate end.
  • Light mineral particles (quartz, altered gangue) remain in the upper layer and are carried mainly by the cross water.
    Finally, particles of different densities and sizes leave the deck in radial bands from edge A toward edge B, discharging at the concentrate end, the middlings zone and the tailings side, and separating precisely into gold concentrate, middlings and tailings. Gold-bearing middlings can be recirculated for re-selection, while in the gold recovery from tailings and precious metals flowsheet the tailings are sent to the tailings dam in line with the gold plant's environmental requirements.

The riffles on the deck are the key to stratification and banding: wash water creates a return flow in the channels that lifts and carries away light minerals, while high-density gold minerals stay at the channel bottoms and migrate progressively toward the concentrate side. Therefore the matching of stroke, stroke frequency, cross slope and wash-water flow directly determines gold recovery and concentrate grade.

Schematic of the 6-S shaking table deck riffles and radial banding of concentrate, middlings and tailings6-S shaking table riffles and radial banding diagram (gold concentrate end·middlings zone·tailings side)

Advantages and Features

  • Extremely high separation precision: a high enrichment ratio (concentrate grade / feed grade) delivers final concentrate and final tailings in a single pass, with outstanding selection efficiency. It strongly captures liberated free gold and coarse-to-medium native gold, making it the key machine for obtaining high-grade concentrate in gold gravity concentration.
  • Flexible operational adjustment: stroke, stroke frequency, cross slope and wash-water flow can all be conveniently adjusted to suit different gold ore natures (auriferous quartz veins, altered rock, placers) and size fractions.
  • Multiple decks available: three distinct decks—coarse sand, fine sand and slime—with different riffle sections, and a light, wear-resistant material such as fiberglass can be selected to meet the separation requirements of different fractions, serving both gold-sand recovery and slime recovery after grinding.
  • Stable, reliable operation: the compact design with springs housed inside the box ensures stable running and maintains balance even when adjusting the stroke; its robust structure and long service life suit the prolonged continuous duty of gold plants.
  • Easy operation and maintenance: simple operation, convenient maintenance and a low failure rate; no chemical reagent is added at any stage, so gravity gold concentrate can pass directly to the next concentration stage, to an alternative to mercury amalgamation, or to smelting.
  • Economical and environmentally friendly: low energy and water consumption per unit of capacity, a compact footprint, and easy incorporation or replacement in an existing gold plant circuit; frequently used in plant upgrades to improve recovery.
On-site installation of a bank of 6-S shaking tables in a gold plantOn-site installation of the GoldProcessingPlant 6-S shaking table selection bank in a gold plant (multiple units in parallel)

Applicable Minerals and Size Fractions

  • Applicable minerals: tungsten, tin, tantalum, niobium, gold, silver, iron, manganese, chromium, titanium, bismuth, lead, zinc and coal, among others. In the gold sector it suits recovery of free gold and middlings after grinding of hard-rock deposits (auriferous quartz veins, altered rock, silicified fracture zones), washing and upgrading of placer gold and river-sand-associated gold, and reprocessing of old tailings and gravity concentrates.
  • Effective size range:
    • Coarse sand: 2 - 0.5 mm (for coarse placer gold and rough gravity concentrate of hard-rock ore).
    • Fine sand: 0.5 - 0.074 mm (the main recovery fraction after grinding of auriferous quartz veins and altered-rock deposits).
    • Slime: < 0.074 mm (for scavenging ultrafine gold and auriferous slime, reducing tailings losses).
    • *For tungsten and tin treatment, the effective recovery range is 2 to 0.022 mm.
Detail of the deck and riffles of a 6-S shaking table6-S shaking table deck and riffle detail (selectable coarse sand / fine sand / slime riffle sections)

Technical Specifications

Model and parameter 6-S 7.6 6-S 4.08 6-S 1.95 6-S 0.5
Deck type Coarse sand / fine sand / slime Three options Three options Three options
Deck area (m²) 7.6 4.08 1.95 0.5
Feed size (mm) Coarse sand: <2
Fine sand: <0.5
Slime: <0.074
<2 (sand)
<0.074 (slime)
<2 (sand)
<0.074 (slime)
<2 (sand)
<0.1 (slime)
Capacity (t/h) Coarse sand: 1-1.2
Fine sand: 0.5-1
Slime: 0.3-0.5
0.4-1.5 0.3-0.8 0.05-0.2
Stroke (mm) 16-22 / 11-16 / 8-16 6-30 12-28 9-17
Stroke frequency (r/min) 220 / 250 / 280 210-320 250-450 280-460
Water consumption (t/h) 0.7-1 / 0.4-0.7 0.3-1.5 0.2-1 0.1-0.5
Motor power (kW) 1.1 1.1 1.1 0.55

Note: according to feed position, each model can be supplied in left-hand or right-hand configuration to facilitate plant circuit layout.

Gold mine selection recommendation: the large-deck 6-S 7.6 (coarse sand 1-1.2 t/h per unit) is suitable as the main cleaning and scavenging bank in medium and large plants, with several units in parallel matched to the gravity circuit capacity. The 6-S 4.08 and 6-S 1.95 are commonly used for free-gold cleaning and middlings reprocessing in small and medium hard-rock gold mines (auriferous quartz veins, altered rock). The small-deck 6-S 0.5 is mainly used in gold test lines, laboratory flowsheet studies or small placer washing banks with limited space. Placers with feed size above 0.5 mm should use a coarse-sand deck; hard-rock deposits ground to -200 mesh should use a fine-sand or slime deck. GoldProcessingPlant can freely recommend deck type, model and number of parallel units based on capacity, grinding fineness and circuit position.

Shaking table gravity concentration in placer and hard-rock gold plantsShaking table gravity concentration in placer and hard-rock gold plants (roughing—cleaning—scavenging)

Why Choose Our 6-S Shaking Table

  1. Classic and reliable: a widely validated classic design, one of the most used table models worldwide, with many long-term operating cases in gold plants across different countries.
  2. Precise and efficient: unmatched separation precision, the final guarantee of high-grade concentrate; good capture of free gold and coarse-to-medium native gold, effectively lowering gold grade in tailings.
  3. Flexible and versatile: multiple specifications and deck types cover the whole flow from roughing to cleaning and from sand to slime; left- and right-hand configurations facilitate gold plant circuit layout.
  4. Economical and durable: low energy and water consumption, a robust durable structure, minimal maintenance cost and a high return on investment; with no reagents added, downstream gold concentrate treatment is simpler.
  5. Complete-line supply: together with the jaw crusher, spring cone crusher, ball mill, hydrocyclone, jig, centrifugal concentrator and spiral chute, it forms a complete gold mine circuit of crushing—grinding—classification—gravity concentration—flotation from the gold processing equipment list. GoldProcessingPlant provides full support from beneficiation test to installation and commissioning.
Detail of the slope adjustment mechanism and spring box of a 6-S shaking table6-S shaking table slope adjustment mechanism and spring box detail (stable operation, easy stroke adjustment)

Frequently Asked Questions

What is a 6-S shaking table and what role does it play in gold beneficiation?

The 6-S shaking table is a high-precision gravity separator that, through the combined action of gravity, cross-flow water drag, deck friction and reciprocating inertia, stratifies particles by density and size into radial bands, producing concentrate, middlings and tailings in a single pass. In gold plants it is mainly used to recover liberated free gold, native gold and coarse-to-medium gold, performing roughing, cleaning and scavenging; it is the key machine for obtaining high-grade gold concentrate, reducing tailings gold grade and improving overall gold recovery.

Can a 6-S shaking table recover free gold and ultrafine gold from gold ore? What size is required?

Yes. The coarse-sand deck suits 2 - 0.5 mm, the fine-sand deck 0.5 - 0.074 mm, and the slime deck material below 0.074 mm. For native gold liberated after hard-rock ore grinding, the fine-sand deck performs best; for ultrafine gold and auriferous slime, the slime deck is chosen for scavenging to reduce gold-slime losses. If the gold is heavily locked, GoldProcessingPlant should first determine the liberation size by grinding-fineness tests and only then define the deck type.

How do I choose between coarse-sand, fine-sand and slime decks?

Choose by feed size and duty position: material above 0.5 mm such as placer gold and jig rough concentrate uses a coarse-sand deck; ground and classified products of auriferous quartz veins and altered-rock deposits (typically -0.5 mm with a high -200 mesh fraction) use a fine-sand deck; slimes below 0.074 mm such as hydrocyclone overflow and centrifugal concentrator tailings in the gravity separation circuit for hard-rock gold ore use a slime deck. A single 6-S table model accepts interchange of all three decks, and GoldProcessingPlant can recommend the configuration based on beneficiation tests.

Where is the 6-S shaking table installed in a gold circuit?

There are three common positions: first, after placer washing and screening (washing trommel, jig) for roughing and cleaning; second, after the hard-rock ore grinding and classification circuit (ball mill—hydrocyclone) for gravity concentration and free-gold recovery; third, over the tailings or middlings of centrifugal concentrators, sluices and gold carpets for scavenging and recovering ultrafine gold once more. In old gold plant upgrades the table is also used to replace obsolete processes and raise overall gold recovery.

How does table gold concentration differ from jigs and centrifugal concentrators? Can they be used together?

A jig has large capacity and excels at roughing coarse and medium gold; a centrifugal concentrator excels at pre-concentrating ultrafine gold; the 6-S table excels at high separation precision and a large enrichment ratio, and is used to turn rough concentrate into a high-grade final gold concentrate. They are complementary, and gold plants commonly adopt the combination of "jig or centrifugal concentrator for roughing and pre-concentration + table for final cleaning", reconciling capacity with concentrate grade. GoldProcessingPlant can propose a gravity equipment combination to your ore nature; see also the washing trommel option.

What is the capacity of a 6-S shaking table? How many tables does a 50 t/h plant need?

Single-unit capacity by model is 0.05-1.2 t/h (the 6-S 0.5 is 0.05-0.2 t/h; the 6-S 7.6 with coarse sand can reach 1-1.2 t/h), so the table is a cleaning machine and must be installed in banks of several parallel units. In the gravity section of a gold plant of about 50 t/h, the number of parallel units is calculated from feed quantity and density and the target concentrate grade; typically a jig or centrifugal concentrator greatly reduces the volume before the table performs final cleaning. GoldProcessingPlant can issue a model and table-count configuration table based on capacity.

How are the stroke, frequency, slope and wash water of the table adjusted?

The 6-S table stroke can be adjusted over 6-30 mm (the 6-S 7.6 corresponds to 16-22 / 11-16 / 8-16 mm by deck type), the frequency is 210-460 r/min, and both cross slope and wash-water flow are adjustable. A general rule: coarse gold and a coarse-sand deck use a large stroke, lower frequency and greater water flow; fine gold and slime use a small stroke, higher frequency and less water. After adjustment, gold grades at the concentrate end and in tailings stabilize markedly, and GoldProcessingPlant can offer on-site start-up parameter recommendations.

Does a 6-S shaking table consume much energy and water? What are the operating costs?

Very little. The 6-S table motor power is only 0.55-1.1 kW and water consumption per unit is 0.1-1.5 t/h, and it can be connected to the plant water recirculation system. The machine has no complex hydraulic or pneumatic systems and adds no chemical reagent; day-to-day work only requires checking the spring box, slope adjustment mechanism and feed uniformity. For a gold plant, the table is one of the precision separators with the lowest operating cost per tonne and offers a high return on investment.

What wear parts does a 6-S shaking table have? How is it maintained? What do left-hand and right-hand mean?

The main wear parts are the deck (replaceable with a fiberglass or wear-resistant deck when riffles wear), the transmission parts of the shaking mechanism and the springs, and the feed and water distribution pipes. Daily maintenance focuses on keeping feed uniform, cleaning deck scale promptly, checking spring compression and bolt tightness, and ensuring stable wash-water pressure. Left/right means the feed end is on the left or right side of the deck; it only affects circuit layout direction, not separation indices, and the gold plant can choose according to its workshop layout.

How much does a 6-S shaking table cost? What information is needed for a quotation?

The price depends on model (6-S 7.6 / 4.08 / 1.95 / 0.5), deck type (coarse sand / fine sand / slime), deck material (fiberglass or traditional), left- or right-hand configuration and the number of parallel units. Provide the gold plant capacity, ore type (auriferous quartz vein / altered rock / placer), grinding fineness and duty position (roughing, cleaning or scavenging); GoldProcessingPlant beneficiation engineers can match the model and unit count and freely issue the quotation and gravity circuit layout proposal.

The 6-S shaking table is an indispensable high-precision gravity separator in the modern gold plant. Although single-unit capacity is limited, its outstanding separation precision, high enrichment ratio and flexibility of deck and operational adjustment make it irreplaceable in free gold recovery, gold concentrate upgrading, placer washing and old tailings reprocessing, serving as an important tool for improving the technical and economic indices of the whole gold beneficiation flow. Based on your gold ore nature, capacity and target concentrate grade, GoldProcessingPlant can provide the optimal table selection and a complete crushing—grinding—classification—gravity concentration—flotation solution.

Tell Us Your Gold Ore Capacity and Grinding Fineness

GoldProcessingPlant beneficiation engineers will match the right 6-S shaking table model, deck type and number of parallel units for your circuit

We freely provide selection and quotation, with complete-line supply of jigs, centrifugal concentrators and ball mills

Get 6-S Shaking Table Selection and a Quotation

CONTACT US

To find out more about our products and solutions, please fill out the form below and one of our experts will get back to you shortly.

Nginx server needs to configure pseudo-static rules, click View configuration method