100 TPD Rock Gold Processing Plant: Flotation & Cyanidation Equipment
100 TPD Rock Gold Processing Plant: Flotation & Cyanidation Equipment
For small to medium-scale rock gold mining projects with a capacity of 100 tons per day (100 TPD), the key to a high Return on Investment (ROI) lies in "precise equipment selection" and "process matching." Specifically for sulfide primary gold ores with low silt content that are easy to concentrate via flotation, the Flotation-Concentrate Cyanidation combined process is currently the best choice to balance high recovery rates and low operating costs. This article details the core equipment list, process flow, and technical parameters for a 100 t/d rock gold processing plant, helping you avoid investment risks in the early stages and achieve efficient gold extraction.
I. Why is the "Flotation-Concentrate Cyanidation" Process Preferred for 100 TPD Plants?
When consulting on building a 100 tons per day processing plant, many mine owners ask: "Should my gold mine use flotation or all-sliming cyanidation?" For a 100 TPD sulfide primary ore, if the gold is hosted in pyrite or arsenopyrite, direct all-sliming cyanidation will lead to massive reagent consumption and extremely high costs. Adopting the 100 t/d flotation-cyanidation process offers three core advantages:
- Lower Investment & Operating Costs: After flotation concentration, the ore volume entering the cyanidation circuit is greatly reduced. This not only shrinks the size of leaching tanks but also significantly lowers cyanide consumption. For a 100 TPD plant, this greatly saves infrastructure investment.
- Higher Concentrate Grade: The selected gold concentrate has a high grade, which is beneficial for subsequent cyanidation or direct shipment to a smelter, achieving "on-site gold concentration."
- Less Environmental Pressure: Tailings volume is reduced, and acidification can be used to treat barren solution (recovering over 70% of cyanide), significantly lowering environmental risks.

100 TPD Rock Gold Flotation-Concentrate Cyanidation Process Flowchart
II. Main Equipment List for 100 Tons Per Day (100 TPD) Rock Gold Plant
Reasonable equipment matching is the prerequisite for ensuring the 100 tons per day capacity. It must be emphasized that the configuration of processing equipment highly depends on the specific properties of the ore (such as hardness, dissemination size, and silt content). The list below is a 100 TPD reference equipment list compiled by GoldProcessingPlant based on years of EPC turnkey experience, utilizing the typical sulfide gold flotation-cyanidation process. In actual projects, our engineers will tailor and optimize the equipment models, quantities, and specifications based on your ore sample assay results. This ensures the full process—from crushing to smelting—perfectly matches your budget and site conditions.
| Process Stage | Equipment Name | Model & Specs | Qty (Sets) |
|---|---|---|---|
| Crushing & Screening | Jaw Crusher (Coarse) | PE250×400 | 1 |
| Crushing & Screening | Cone Crusher (Fine) | PB600 | 1 |
| Crushing & Screening | Circular Vibrating Screen | ZD0612 | 1 |
| Grinding & Classifying | Spiral Classifier | FG-10 | 2 |
| Grinding & Classifying | Grate Ball Mill | MQZ1530 | 1 |
| Flotation | Flotation Machine (Rougher/Scavenger/Cleaner) | XCF/KYF-1 | 20 |
| Flotation | Overflow Ball Mill (Regrinding) | MQYZ1224 | 1 |
| Thickening & Leaching | Single Deck Thickener | NZ-6 | 1 |
| Thickening & Leaching | Agitation Tank (Leaching) | SJ2×2.5 | 10 |
| Thickening & Leaching | Three-Layer Thickener | 3NZ-6 | 2 |
| Substitution & Smelting | Decoxidation Tower | TY1030 | 1 |
| Substitution & Smelting | Zinc Powder Feeder | CH140 | 1 |
| Substitution & Smelting | Filter Press | YL30 | 1 |

III. Core Process Flow & Technical Parameters of the 100 TPD Plant
In the standard Raw Ore → Jaw Crusher → Cone Crusher → Screening → Ball Mill → Flotation → Regrinding → Thickening → Leaching → Substitution process, the following stages determine the success of a 100 t/d project:
1. Grinding & Flotation Concentration
The 100 tons per day plant uses a grate ball mill (MQZ1530) for coarse grinding, combined with XCF/KYF flotation machines (20 sets) for roughing, scavenging, and cleaning. The rough concentrate from flotation enters an overflow ball mill (MQYZ1224) for regrinding, ensuring the full liberation of gold minerals.
2. Cyanidation Leaching & Substitution (Technical Specs)
This is the core of gold extraction for 100 TPD. The slurry entering the leaching tanks (SJ2×2.5, 10 sets) must meet the following strict parameters:
- Grinding Size: 98% passing 400 mesh (extremely high liberation).
- Leaching Time: 36 hours (ensures sufficient dissolution).
- Cyanide Consumption: 3.5 kg/t of concentrate.
- Extract Concentration / Wash Water Ratio: 0.15-0.2% / 1:4.
- Final Targets: Leaching rate 97%, washing rate 99.5%, substitution rate 99.5%, total cyanidation recovery rate 95.5%.
The pregnant solution after leaching is deoxygenated through a decoxidation tower (TY1030), replaced by zinc powder (via CH140 feeder), and finally pressed by a filter press (YL30) to obtain gold slime, which is sent to the smelter.
IV. Equipment Selection Pitfall Guide for 100 TPD Plants
Building a 100 tons per day processing plant, the biggest risk isn't paying too much, but "buying the wrong thing." Here are the top three pitfalls we've summarized from serving global mining clients:
- Pitfall 1: Blindly copying others' drawings. No two rocks in the world are exactly the same. Even for the same 100 t/d capacity, the equipment configuration for oxide and sulfide ores is vastly different. You must conduct ore dressing tests first to understand the dissemination size and sliming degree.
- Pitfall 2: Skimping on grinding equipment to save small money. Although 100 TPD is a small scale, grinding is key to achieving mineral liberation. If the matching of the grate ball mill and the classifier is insufficient, the subsequent flotation and leaching rates will never reach 95.5%.
- Pitfall 3: Ignoring civil engineering and installation adaptability. Many clients piece together equipment themselves, causing piping clashes and mismatched equipment foundations. GoldProcessingPlant provides full services from process design to 3D drawings, ensuring perfect equipment-site alignment.

V. Why Global Miners Choose GoldProcessingPlant for 100 TPD Plants
Factory Direct, No Middleman Markup
We have two proprietary manufacturing bases in Shandong and Jiangxi. The full set of 100 TPD plant equipment (from crushing to filter pressing) is shipped directly from the factory. This ensures controllable delivery times (60-90 days for standard equipment) and highly cost-effective pricing.
Seamless Process & Mechanical Integration
Process engineers and mechanical engineers work collaboratively in the same team. The design drawings for your 100 tons per day plant perfectly match the equipment dimensions, completely eliminating the issue of "disconnected drawings and equipment."
Flexible EPC Turnkey Model
For overseas 100 TPD projects, we recommend: equipment manufacturing, process design, and installation guidance are handled by us; civil works and general laborers are organized locally by you. This ensures technical quality while significantly saving you high labor costs for expatriate workers.
No Project Too Small
Whether it's a 30 t/d pilot line or a 100 t/d, 1000 t/d industrial production line, we treat them equally. Scale only affects equipment configuration and budget, not our high standards for process design.

VI. Frequently Asked Questions about 100 TPD Processing Plants
Get Your Customized 100 TPD Rock Gold Processing Solution
The equipment list above is a standard reference for the 100 TPD scale, but "no two rocks in the world are exactly the same." The dissemination size, silt content, and associated elements of your gold ore determine the final streamlined or enhanced configuration.
Send us your ore samples, and GoldProcessingPlant's mineral processing engineers will issue a "Process Solution Report" within 30-45 days, including a detailed 100 TPD equipment selection, accurate quotation, and expected recovery rate.
Contact us to create greater value from every ton of rock gold ore.